Beautiful Plants For Your Interior

Hydroxyacrylic Dispersion Houxian® 4002L
Product Features
Houxian® 4002L is a waterborne hydroxyacrylic dispersion, suitable for use as a two-component system when formulated with waterborne isocyanate curing agents. Approximately 41% solid content is dispersed in a water/ethylene glycol butyl ether solution and neutralized with dimethylethanolamine. It is recommended for applications such as two-component waterborne wood coatings, industrial coatings and floor coatings. This product has the following features:
- Transparent dry and wet films
- High hydroxyl value
- High hardness
Physical Properties*
| Characteristics | Technical Indicators | Test Methods |
| Appearance | Milky white slightly yellow translucent emulsion | Visual inspection |
| Solid Content (wt%)(140℃, 1g, 30min) | 39-41 | GB/T 1725-2007 |
| Viscosity (25℃, mPa·s) | 100-2000 | GB/T 2794-2022 |
| pH Value (25℃) | 6-8 | GB/T 8325-1987 |
| Hydroxyl Content (based on solid content, wt%) | ~4.2 | GB/T 31412-2015 |
*The performance data presented herein are typical results only and shall not be deemed as specifications. Product specifications shall be subject to the specific Certificate of Analysis (COA).
Packaging Specifications
Plastic drum: 125 KG/drum; 1000 KG/drum
Storage
This product should be stored in a dark, cool and dry place at a temperature of 5–35℃ with the packaging kept intact. The shelf life of this product is 12 months from the date of production. For products beyond the shelf life, performance evaluation is recommended prior to use. This product must be strictly protected from frost and direct sunlight. After opening the packaging, appropriate filtration is recommended before use, and the product should be used up as soon as possible.
Precautions for Use
- Stir thoroughly before use and seal tightly after use. Do not mix with cationic substances or inks.
- The viscosity of this product is mainly affected by the pH value. The pH value may decrease during storage, and the product viscosity will decrease accordingly. Its viscosity can be adjusted back to the initial value by adding a small amount of 10% aqueous N,N-dimethylethanolamine solution.